Deterioration of sandstones: Insights from experimental weathering in acidic, neutral and biotic solutions with Acidithiobacillus thiooxidans

Vorschaubild nicht verfügbar
Autor:innen
Potysz, Anna
Bartz, Wojciech
Zboińska, Katarzyna
Autor:in (Körperschaft)
Publikationsdatum
24.02.2020
Typ der Arbeit
Studiengang
Typ
01A - Beitrag in wissenschaftlicher Zeitschrift
Herausgeber:innen
Herausgeber:in (Körperschaft)
Betreuer:in
Übergeordnetes Werk
Construction and Building Materials
Themenheft
Link
Reihe / Serie
Reihennummer
Jahrgang / Band
246
Ausgabe / Nummer
Seiten / Dauer
Patentnummer
Verlag / Herausgebende Institution
Elsevier
Verlagsort / Veranstaltungsort
Auflage
Version
Programmiersprache
Abtretungsempfänger:in
Praxispartner:in/Auftraggeber:in
Zusammenfassung
The susceptibility of sandstones to deteriorative factors when used for construction requires detailed experimental evaluation. This study investigated the (bio)weathering behaviour of Lower-Silesian Cretaceous sandstones (quartz arenites) to quantify the deteriorative effect of bacterium Acidithiobacillus thiooxidans. For controls, ultrapure water (in undersaturated conditions) and sterile acidic medium (in abiotic acidic conditions pH 2.5) were used. Sandstone exposure to A. thiooxidans mimicked the extremely acidic conditions (pH up to 0.9) that may develop under long-term weathering, which promote microbial activity and acidic metabolite production. Element release was assessed using triple quadrupole inductively coupled plasma mass spectrometry (QQQ-ICP-MS) and identifying potential element donor minerals through scanning electron microscopy, coupled with energy dispersive spectrometer (SEM-EDS). The results demonstrated that sandstones were relatively susceptible to weathering, especially when exposed to aggressive acidic conditions, where the presence of bacteria apparently acts as an accelerating factor in deterioration. Based on Si release, sandstone degradation under biotic conditions was 0.27% within 86 days, whereas the dissolution achieved in ultrapure water did not exceed 0.02%. A highly pronounced weathering feature observed on sandstones was the dissolution of goethite and/or kaolinite cement, whereas quartz was less susceptible to weathering under the conditions studied. Bioweathering investigations may help solve deterioration issues in sandstone building materials.
Schlagwörter
Sandstone, Quartz arenites, Bacteria, Bio-weathering, Deterioration, Building materials
Fachgebiet (DDC)
Projekt
Veranstaltung
Startdatum der Ausstellung
Enddatum der Ausstellung
Startdatum der Konferenz
Enddatum der Konferenz
Datum der letzten Prüfung
ISBN
ISSN
1879-0526
0950-0618
Sprache
Englisch
Während FHNW Zugehörigkeit erstellt
Ja
Zukunftsfelder FHNW
Publikationsstatus
Veröffentlicht
Begutachtung
Peer-Review der ganzen Publikation
Open Access-Status
Lizenz
Zitation
POTYSZ, Anna, Felix SCHMIDT, Markus LENZ, Wojciech BARTZ und Katarzyna ZBOIŃSKA, 2020. Deterioration of sandstones: Insights from experimental weathering in acidic, neutral and biotic solutions with Acidithiobacillus thiooxidans. Construction and Building Materials. 24 Februar 2020. Bd. 246. DOI 10.1016/j.conbuildmat.2020.118474. Verfügbar unter: https://irf.fhnw.ch/handle/11654/32383